Beilstein J. Nanotechnol.2022,13, 1020–1029, doi:10.3762/bjnano.13.89
0.94 V vs RHE, 0.78 V, and 3.6 mA·cm−2, respectively, with an electrochemical active surface area of 66.92 m2·g−1 and a mass activity of 40.55 mA·mg−1. The optimum electrocatalyst shows considerable electrochemical stability over 10,000 cycles in 0.1 M KOH solution.
Keywords: coppercobaltoxideNPs
PDF
Figure 1:
Illustration of the formation of AgCoCu oxide NPs over rGO with tuneable Ag fractions.